ASTM A335 is the specification behind most high-temperature alloy piping you will ever quote: seamless ferritic alloy steel pipe intended for high-temperature service, covering the chromium-molybdenum grades from simple carbon-moly up to the 9% chromium creep-resisting steels. The "P" in P11, P22 or P91 simply means pipe; the same chemistry in tube form carries a "T". Because the standard spans several very different families, the real buying decision is rarely "A335 or not" - it is which grade, in which heat treatment condition, with which test menu. This page is the family overview; each grade we ship has its own page with chemistry, fabrication notes and ordering details.

Choosing the Grade: What Each P-Number Is For
Grade selection follows metal temperature, not pressure alone. The chromium in the alloy does two jobs - it slows oxidation and it resists hydrogen attack - while molybdenum holds creep strength at temperature. More chromium buys higher temperature capability at the cost of harder welding and stricter heat treatment, which is why the jump from P22 to P91 changes fabrication practice, not just price.
| Grade | Nominal chemistry | Typical service temperature | Where it earns its keep |
|---|---|---|---|
| P11 | 1.25 Cr - 0.5 Mo | up to about 500 degrees C | Steam mains, boiler tubes, exchanger shells |
| P22 | 2.25 Cr - 1 Mo | up to about 550 degrees C | Reheater and header piping, refinery furnace lines |
| P91 | 9 Cr - 1 Mo - V, Nb | up to about 600 degrees C | HRSG and combined-cycle main steam |
| 16Mo3 (EN 10216-2) | 0.3 Mo | up to about 450 degrees C | European boiler and pressure vessel work |
Table note: temperature limits are indicative design ranges. Actual allowable stress depends on the design code and the temperature line on your datasheet.
A working rule for a first pass: if the drawing says carbon steel will not survive but the temperature stays below 500 degrees C, P11 is the default answer. Between 500 and 550, P22. Above that, P91 unless the whole system is European, in which case the designer may have written 16Mo3 for the cooler circuits and an X-series grade for the hottest ones. When the choice is genuinely close, the deciding factors are usually welding capability at the fabricator and the lifetime creep data behind each grade - see our P11 alloy steel pipe, P22 alloy steel pipe and P91 alloy steel pipe pages for the detailed comparison.
Sizes and Manufacturing Range
A335 pipe is seamless, produced by hot piercing and rolling, hot drawing or cold drawing depending on size and tolerance demand. The practical envelope we quote runs from about 21.3 mm OD (half inch) up to 711 mm (28 inch) with wall thickness from schedule 10 through schedule 160 and heavier by agreement. Standard lengths are 6 m and 12 m random, with fixed lengths cut to order. Beyond about 24 inch, seamless alloy becomes expensive enough that many projects shift the large sizes to welded alternatives and keep A335 for the critical small and medium bore - worth deciding at design stage rather than at quotation.
Tolerance matters as much as size. A335 references ASTM A530 for outside diameter and wall tolerances, and cold drawn sizes can be held to tighter limits where the application needs them. If your fabrication uses orbital welding on thin wall, say so at inquiry: the difference between a standard-tolerance and a close-tolerance heat is visible in fit-up time within the first shift.
Heat Treatment and the Test Menu
Every A335 grade must be supplied heat treated, and the required condition differs by grade: P11 and P22 are normalized and tempered, P91 is normalized and tempered with tightly controlled tempering parameters, and the carbon-moly grades are normalized. The mill certificate must show the actual treatment temperatures, not just the words. On top of the standard tension and hardness tests, the common add-ons are impact testing at a stated temperature, ultrasonic examination to ASTM A999 or EN equivalents, and hydrostatic testing. For refinery work in hydrogen service, buyers also ask for elevated temperature tensile values on the certificate.
Certification is where cheap offers separate themselves from workable ones. We ship with EN 10204 3.1 certificates tied to heat numbers, and we support 3.2 third-party witness where the project demands it. If you are cross-checking an offer, the fastest filter is to ask the supplier for a sample MTC from a recent A335 heat - the treatment temperatures and the traceability tell you more than any website. The same discipline applies on the plate side of the same alloys, which we cover under ASTM A387 Grade 11 alloy steel plate for vessel fabrication.
What to Confirm Before You Place the Order
Three things prevent most A335 disputes. First, freeze the grade and the size schedule in writing together, because P22 ordered where P11 was meant is a real and expensive mistake - the grades look identical on a warehouse rack. Second, agree the heat treatment condition and the certificate contents before production, not after inspection. Third, agree packing and length mix: mixed 6 m and 12 m lengths in one container change the loading plan and the freight per tonne. Our service page lists how we handle heat treatment records and export packing, and the https://www.henry-china.com/faq covers documents; for grade-level detail start with seamless alloy steel pipe for how the sizes are actually made.
Is A335 always seamless?
Yes - A335 covers seamless pipe only. If a project allows welded alloy pipe, the applicable specification is different (A691 for electric fusion welded), and the weld procedure and PWHT requirements change with it.
What is the difference between P11 and T11?
Chemistry is the same. P grades are pipe under A335, T grades are tube under A213, used inside boilers. Wall tolerance and test frequency differ slightly, so the two are not interchangeable on paper even when the metal is identical.
Can you supply A335 with third-party inspection?
Yes - SGS, BV, TUV or the inspector your project names, witness testing at the mill, with 3.2 certificates issued against witnessed results. Inspection booking is easier when the request comes with the purchase order rather than after production.
How fast can A335 be quoted and shipped?
Stock sizes quote within a working day; production sizes typically run four to ten weeks depending on grade and heat treatment queue. Transit planning is covered in our note on steel pipe lead time from China.
Hot Tags: astm a335 alloy steel pipe, a335 p11 pipe, a335 p22 pipe, a335 p91 pipe, high temperature alloy steel pipe, a335 seamless pipe China supplier, alloy steel pipe price